iron ore beneficiation plant and circuit study in iran The two main methods of recycling iron from iron ore tailings are magnetizing roasting and direct reduction Magnetizing roasting uses temperatures between 700 and 900 °C for a time of under 1 hour to produce an iron concentrate Fe 3 O 4 to be used for iron